Paul Merica patents the first superalloy
From ETHW
In 1926, Paul Merica patented the addition of small amounts of aluminum to Ni-Cr alloy to create the first "superalloy." This led to the commercialization of the jet engine, along with increased efficiency for modern power turbine machinery.